Quote:
|
Originally Posted by jrow
If the holes "pits" aren't to deep the powder will cover them, and yes you may need multiple coats. With deeper holes / road rash use Arvin's Lab Metal. Some have used JB Weld with good success!
John
|
JB Weld rocks. I've used it to replace a stripped-out exhaust manifold bolt hole in a '51 dodge flathead six, and it held up great. So I know it'll take the heat. Good idea.