Takes so long?
I was just wondering I am working on a aluminum piece.It is sandblasted first,then sanded, then flash coppered,then acid copper.It take so long to fill all the scratches,How do the professional shops do it so quick,Does cyinide copper plate faster and thicker than the copper we use.How can you make any money when it takes you 16 hrs(or more), to chrome plate a 4 x 9 piece of aluminum?.When a chrome shop only charges $150.00 to do it?. Thanks for your input.
|