Quote:
Originally Posted by Popeye
We use a coil cleaner to etch our parts.. should be able to pick up a gallon at the local HVAC place or HVAC supply house.
You'll want to degrease the parts before dipping.. usually about 45 secs in the bath does the trick.. your mileage may vary
After the bath, do you follow up rinse it?