It may look the same and all that. But what would have happened if you tried to return it on Ebay. Besides, the support here is as good as the rest of Caswell stuff. It took me a few times to get the hang of the Caswell, as I also have an EW Hobby gun and have had that one for sometime. I like having the higher voltage, but like them both. If the powder isn't sticking, could it be a bad ground or something along those lines?