I received the 4 gallon triple chrome plate kit. Was I suppose to receive the pickle #4 salt crystals? I received two bags of the SP degreaser. Without paying any attention, I dumped and mixed both bags in 4 gallons of distilled water

I then noticed on the bag that is says to mix one pound with two gallons and one bag was two pounds so when I dumped both bags in, I now have a double wammy of SP degreaser!! Easy enough to fix....just mix another 4 gallons in it and all is well. What would happen if I use the SP degreaser in that concentration though? Was one of those SP degreaser salt bags suppose to have been the pickle #4 salts?