View Single Post
  #11 (permalink)  
Old 05-17-2007, 02:03 PM
Banditperformance Banditperformance is offline
Metal Finishing Guru
 
Join Date: Jun 2006
Posts: 619
Banditperformance is on a distinguished road
Default Re: Temperature Time to Rise Calculator

It seems a little fast compared to my oven in reality. My oven takes about 45 min to heat to 400, But then, that's with 100+ metal silhouettes inside too. The spreadsheet said 34 min so 10 min off aint that bad at all.
__________________
Dan Pesonen
Bandit Powder Coat <<From Powder to Perfection>>
Forest Grove, BC Canada

Personal motto:
"If it ain't broke, modify somethin till it is"
Reply With Quote