View Single Post
  #7 (permalink)  
Old 05-20-2007, 12:40 PM
outcastzeroone outcastzeroone is offline
Amateur Metal Finisher
 
Join Date: Aug 2005
Posts: 50
outcastzeroone
Default Re: got some questions (dont we all)

you dont think that the 3 short elements would over back the area right over them? the oven will be over 3' long by 2' deep and the elements are 11 3/4" long. I know i would need the ceramic holders for the coil i posted, i just didnt mention that. kinda figured it was a given :P I just want to make sure that i dont over bake part of my parts and kill them. some of the parts will just barely squeze into this oven. I cant justify making it larger since there are only about 3 parts i will be doing but lots of little ones.

And since you mentioned it, anyone know of a good source for insulation and wire to hook up the elements?
Reply With Quote