Default I can't polish my stainless exhaust..

Hi friends, i just bought a stainless steel kit. Im trying to polish my bike's exhaust to a mirror finish like before. Instead of making it shine im making it worst.

How do i polish with e buff wheels? In any directions? For every direction i buff my exhuast will have lots of zig-zag marks on it cause by the sisal wheel/black compound. By the way do i just use a wet cloth to clean away the compound before i change to another? Or i must use soap or something?

Sorry for asking so much at a time. Really new to this..My exhaust is now all hazy marks..Sad.