Don't use a sisal wheel unless you're trying to take out deep scratches. If all you're trying to do is buff out "hair lines", use a cotton buff. When you get the sisal marks out, go to white compound on a new buff. If you want, you could use an SS compound on a another cotton buff as a final. Don't mix compounds on the same buff. Use a separate buff for each compound. Screed often and at the end of your buffing. Store the buffs separate.

The residual compound can be removed with soft rag dipped in naptha or paint thinner. Or it can be removed with car, SS or chrome polish.