carefull with the A arms if they have balljoints like the banshee A arms.
I had an A arm ball joint exploded in my oven outgassing at 450 .
it was a huge explotion and the ball joint stabed my oven wall.
i don't even want to think what can happend if it explodes getting it out of the oven.
also some kind of plastic comes off from inside of the balljoint and they last about 1 year .