Quote:
Originally Posted by tbreaden
You guys are talking about electro-stripping. Where do you get your info? Look at Caswell Plating Manual pg. 30
Nope. It's not electro-stripping! That's "de-plating". This process is simply a conversion. No metal is lost or transfered.