Default had a simular problem with my first attempts

Ok, this may sound dumb, but it got me good for 3 days before I finally worked it out.

Turns out my power supply, a temporary loaner from work, was cutting out around every 5 minutes. It was only by pure fluke that I was watching the needle and heard a faint click and saw the needle flicker. I tried a different supply and all was good. No more flaking problems.

Mark