Well if I wanted to use chemicals to strip the nickel off my brass items am I correct to say that I would use muriatic acid mixed with distilled water. Would this work? Or using muriatic acid mixed with distilled water and a lead anode reversing the wires? All help is greatly appreciated!!!

Also I am using the electroless nickel plating kit and once the nickel is stripped then I can go ahead polish to a high shine and then clean the metal of all debree and plate the part correct?