If you're going to electroless nickel plate it, then I'd just buff it all out and then plate it. Why bother taking the old nickel off if you can just plate over it with nickel again?
Just be sure to have a high polish on it and make sure any areas where the old nickel meets the bare brass is smooth as possible.
|