Default Re: Can I PC this head?

Ya, I wouldnt be worried with that head, Nor about seats loosening. Combustion temps way hotter than curing temps, and that head should not warp, because you are heating it evenly, and only to 400. Heads see temperature Gradients of thousands of degreed between the water jacket and the combustion chamber.
__________________
Dan Pesonen
Bandit Powder Coat <<From Powder to Perfection>>
Forest Grove, BC Canada

Personal motto:
"If it ain't broke, modify somethin till it is"