I noticed on the website that you can individually buy 300W titanium or 50W ceramic heaters with or without a thermostat. It says that the thermostat only controls in a range of 110-140 though.The electroless nickel kits say that they come with 300W ceramic (not titanium) heaters. Doesn't Electroless need to be up around 180degF? I am assuming that the heaters will hit this range without a thermostat, but I wanted to make sure. I'm just a little confused by the different information. Can anyone clarify?

-Nick