That was an option i considered.Problem is,there's a insulated shelf that goes in the middle so that top half can be run by itself.About half of what i do fits in the top half.Had i had it to do over i would have placed the top elements on the side but at this point thats a lot of work.hoping solution can be found to move enough air with out blowing off the powder.