View Single Post
  #4 (permalink)  
Old 06-06-2007, 01:34 PM
cbrooks's Avatar
cbrooks cbrooks is offline
Caswell Inc Staff
 
Join Date: Dec 2003
Posts: 1,086
cbrooks is a glorious beacon of lightcbrooks is a glorious beacon of lightcbrooks is a glorious beacon of lightcbrooks is a glorious beacon of lightcbrooks is a glorious beacon of lightcbrooks is a glorious beacon of light
Default Re: Copy Chrome Setup Need Help Please

When setting up your copy chrome tank the directions on the crystals state to heat, allow to cool then add the brightener. If after copper plating you notice any defects then buff them out before proceeding to the copy chrome. Thoroughly clean the part again making sure that it passes the water break test before going on. Your amps should be set using one amp per 32 square inches. Then the plating time should be for 90 minutes to get a good plating thickness.
__________________
--
Craige Brooks
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com