Default Help Rust under clear coat..

Hello,

I got my motorcycle fenders/gas tank pc'd.

Colors are satin black and bare steel with a satin clear.

Now 3 weeks later i notice this. It is because it is bare steel with a clear over top or what is causing this. Also can i put satin clear over bare metal and have it not rust??