Quote:
Originally Posted by bucky685
Thanks, i figured that it was the prep work that was done on it.

Can finger prints cause a piece to start rusting.

Also the rust was not there to begin with it was a fender off of an 06..
any humidity ,oil , or acid on your skin will affect the metal . alo being from a 2006 has nothing to do with it as soon as your metal has been stripped ,sanded or blasted, oxidation starts .the better you clean and the fastest you coat it better are your chances that rust ill stay away longer