Default Re: Polishing Chrome

Parts are from a Harley, base metal I assume is steel. I'm using a machine at 3,000 rpm with white bar followed by the blue and then "Blue Begone" polishing liquid. Tried both spiral and loose wheels. Changing wheels with each compound and washing the part before applying next compound and wheel. Only thing I think left to try is more speed and pressure