Default Re: Bake from a Cold oven??

Hmm...might be the gun man. I know my EW gun works well...but at $700 it should! It still emits some electrostatic charge at the lowest setting too. Sometimes it sticks too...I just gotta hit the side of the gun and it stops. No buildup in the barrel tho. I get alot of the picture framing effect on totally flat, square surfaces tho. Sometimes I try to shoot everything hot and hit the trigger like I am touching up the part but coating it little by little.