Default Re: Is too much wattage a bad thing?

seems to me, tho i do not know if it holds true in practice, if you have 6000watts and it heats up in 30 mins or 12000watts and it heats up in 15 mins, the cost to run should be the same. and once to temp, they should cycle on/off to maintain temp, which again, should be half as long w/ 2x the power.

i put 2 sets of 2 elements in mine (2800w each). i can either run all 4 or just two, depending on how well it works.