Default Re: Its all in the details...

Do a Google on the rolls...we can't discuss others' products on here...they are available in 1/4" but not in finer grits. The homemade stuff is pretty much the only way to get finer grits in that form.

I have to agree on the Cratex but you can always use small felt bobs with greaseless compound for material removal.


Quote:
Originally Posted by mach1canuck
Where did you find the 1/4 diameter rolls?

ANd I used cratex, and I found it only puts a shine on parts, and if there are bumps, it will only make shiny bumps.