I had this problem about 4 months ago. I had not been plating much over the winter, my tank set for about 6 weeks at 40 deg. I have the wheel chroming kit and was told the larger kits like mine are cobalt only. I cleaned tank and found a rusty sludge in bottom. Now I run a filter when plating and remove anodes and clean after every use. Bath temp 70 to 80 deg. and make sure you have a good sealed anode bags. I have not had any problems since. (except plating pot metal) Todd