One thing I have noticed with my gun is that if I use the diffuser on the end, it adds extra charge to the powder. So much charge that I get a 2" spark off the end. I think it's over charging with that much spark. Without it, no long sparks. I have tested this with a few different powders, and with about 6 Lbs. Allways, with difusser, nasty charge, without, nice and consistent.

PS, I only have the Large difuser, because I accidentally threw the other 2 smaller ones out with the packaging the gun came in