Thread: parts cleaner
View Single Post
  #1 (permalink)  
Old 06-25-2007, 04:49 PM
holeshot87 holeshot87 is offline
Amateur Metal Finisher
 
Join Date: Jan 2005
Posts: 103
holeshot87
Thumbs up parts cleaner

does someone know a good parts cleaner. before i powder coat a part i have been using brake cleaner. .is there something easier to use then brake cleaner and better? thanks