View Single Post
  #6 (permalink)  
Old 06-26-2007, 01:16 PM
SLOSteve SLOSteve is offline
Newbie
 
Join Date: May 2007
Posts: 33
SLOSteve is an unknown quantity at this point
Default Re: Best Blast Media

Quote:
Originally Posted by tbreaden
Maybe you can find a local company to do your blasting for you. because you have to get the chrome off and clean the pits out. then I use the MetalX stripper to strip the nickle,you have to heat this to 130-150f with aggitation. It gets you down to the copper and it will eliminate alot of pits (and work)that are not into the pot metal.. Then you can try the pickle #4 it is a deoxider and activator for zink die cast. Todd Breaden
Hi Todd, There is only one shop near my that "says" they do chrome work but they actually send it 300 miles to be done. Would electro-stripping work on pot metal or no? The surface area of my bezel is very small (10")and most of the pits are actually just "bubbling". I just want to make it concours quality. I have the triple chrome kit so I have all of the necessities for getting the job done except a rheostat. I appreciate your help.
Reply With Quote