Re: parts cleaner
Akline base cleaner works real good, this is what you can do, Call a local air conditon suplly house a place where they sell air condition parts, tell them or go by and pick up some "coil cleaner " that stuff works great , you buy by the gallon You then delete it down works real good It will go a ong way ,,, This stuff is what i use,,
|