the airdrill is time consuming. better use a 'mouse sander' ($30 at sears) and starts with 120 after stripping the clearcoat (urethane clearcoat remover $16 areasol) then onto 180, 240, 320, 400, 600 then polish with emory, finish with white bar. i'm currently doing 17" '95 impala ss rims which is a similar factory finish as yours.