Thread
:
Black oxide cloudy
View Single Post
#
2
(
permalink
)
07-05-2007, 01:43 PM
jwilbert
Metal Finishing Guru
Join Date: Apr 2005
Posts: 551
Re: Black oxide cloudy
Chances are the laquer could be the problem.
Try our degreasers or use hot water and dish soap to clean the parts.
If the solution still gives you good results, keep using it.
Last edited by jwilbert; 07-05-2007 at
01:45 PM
.