Thanks guys...
I didn't know that you can't handle the parts for a couple of days!!! I thought that the part was good to go after the chromate dried.
I am using the brightener. I have read conflicting reports on its use. The chromated parts look much better after the brightener, and much more "original." Without the brightener, they just don't look right, and have a matte finish.
The parts I am replating were originally very shiney/gold cad...
|