My name is Layke Rossiello and i have invented a way to powder coat pictures and designs. I believe that i am the only person in the world able to do this at least to my knowledge anyway.
I have a photo gallery at my space so click this link to have a look:
www.myspace.com/theaussiedeuce
If there is anyone else out there who can do it as well please contact me by email: