Thread: Fix Needed
View Single Post
  #1 (permalink)  
Old 07-12-2007, 10:50 AM
donafams donafams is offline
Amateur Metal Finisher
 
Join Date: Apr 2007
Posts: 229
donafams is on a distinguished road
Default Fix Needed

i just powdered a glovebox door from an old car and the front side needs to be redone but the back is ok.. Can i just blast and sand the front or will i need to do the back side also?