Thread: yellow tint?
View Single Post
  #8 (permalink)  
Old 07-23-2007, 11:30 PM
john1951 john1951 is offline
Newbie
 
Join Date: Dec 2006
Posts: 7
john1951 is an unknown quantity at this point
Default Re: yellow tint?

Hi I have the same problem even with the very first items I plated. I followed the temps and amps per the directions . Had the slight yellow tint right after buffing the parts. not as white as real chrome. Some types of lights make it look much wurse than others next to the triple chrome stuff on my bike. I waxed it and still no difference.