Re: PLATING POT METAL...............
AAAAHHHHHH!!!!!
now that I got that out of the way, can somone tell me, after my repairs, I have these tiny holes, over and over, cannot get them out, I'm talking pinholes. will flash copper and then acid copper buildup cover these?
I'm at my wits end, have used solder-it, muggyweld, silver solder, still have the pin holes. blasting, sanding, buffing, cannot get rid of them. have started this piece over about 50 times{no s..t} arrgggg, rotten pot metal.