Default Powder Coat Removal

Today I removed some powder coat with an abrasive blaster. I had never done this before so I didn't know what to expect. What I saw was the abrasive and the air seemed to cause the powder coat to "bubble up" to where you could just kind of peel it off. Now, is this typical of the way powder bonds, or am I having adhesion problems?