my work
i just finished coating this Edelbrock set for a customer. The base coat is safty yellow, the top coat is super high gloss clear mixed with gold sparkle. It is hard to see the gold sparkle in the pictures but in person the gold looks good. just so i am on the same page as every one, what would one charge for a job like this. The parts had to be striped and sandblasted.
|