Originally Posted by sswee
I have the larger unit. Can't remember the number. The only problem, so to speak, was the weak springs in the clamps. Bad connections in the clamps caused arcing in the clamp connection and it burning out the clamp teeth. Just replaced the clamps to fix. No problems with the welder itself. Always worked as it's suppose to.
SS
Thanks sswee, I appreciate your input.
I'll be sure to use good stout clamps on mine.

-