I currently seal with boiling water no problems, i seem to get a nice colour fast surface with about 10-15 minutes in a boiling tank. However since it seems it has nothing to do with being a) out of the air or b) in water, I would have thought you could just throw the item in an oven instead - heating an oven to 100 C or more takes a lot less energy than heating a pan of water to 100C and holding it there for a long period.

? I might try it for the sake of experimentation.