I have a gun now like the Caswell $100 unit. I like mine so far.
I think I been using 1-2" of powder in the cup, not allot but not paying much attention to it, I just dump in a bit and go.
I been doing 10"dia. flat plate steel parts so far, nothing fancy for me yet.