Re: Big quote for us with lotsa Masking
Anyone want to guesstimate how long something like this takes to mask with mask it? I tried using the mask it on a test piece once and it took a forever to do a 1.5" diameter circle, and it was difficult to keep it from getting in a groove next to the mask. Was pretty difficult to remove as well, but I think I read somewhere that lacquer thinner helps in that department. Anyone have tips on best practices while using the stuff?
|