View Single Post
  #24 (permalink)  
Old 07-31-2007, 04:28 PM
luminous's Avatar
luminous luminous is offline
Amateur Metal Finisher
 
Join Date: Jun 2005
Location: smalltown, USA
Posts: 98
luminous will become famous soon enough
Default Re: Sput welder, where can I buy one of these?

Quote:
Originally Posted by LOON
Don't know if this really helps....but I heard something of charge time and welding....
At our signmaking shop we use this one to weld bolts, and stuff to almost any material....mostly aluminium

http://soyer.cc/de/index.php?option=...120&Itemid=163 ok....it's a german site ....but take a look....you'll find an aequivalent product in the U.S.....
Well, that does like like a nice unit! I've used stud welders somewhat similar to that before. But... that would be total overkill I think for what most small time anodizers need, and I'm afraid that the nearly $2700 USD price tag might be little much for my target audience. Neat though. Thanks for the link.

steve

-
Reply With Quote