Default Re: New Anodizer-Tank Set Up Question

Luminous's method works well for small tanks.
HVAC uses a window-mount type AC unit blowing into a box that contains the ano tank. I think his tank is around 20 gal too, and that method works well.
I've heard bad results from the heat-sink type chillers. Personally, I use a 1/4hp titanium core chiller. I've calculated it to chill approx 1500 watts. It barely has enough poop to keep my 50gal tank with 20 amps going through it at temp (I'm in Seattle, and temps are fair).
Looking back, I should have gone with the AC unit... I even had a spare.
__________________