Default Solar Flat Black issues

At work we tried useing some of hte caswell Solar Flat Black on a peice for a car we where working on. It had a couple of shiny spots on it and a booger so we sanded it down and reshot it with the flat and cooked it at 175 for 12 min. Only when we pulled it out it was gloss/semi gloss and not flat at all.

Has anyone had isues useing the Solar Flat Black before? Did we screw up on the second coat?