instructions for plating over lab metal
Instructions for plating parts repaired with Lab-metal:
1. Follow directions for Lab-metal
application.
2. Alkaline cleaner
3. Aluminum etch
4. Deoxidation
5. Zincate
6. Deoxidation
7. Zincate
8. Acid and copper plate
9. Nickel
10. Chrome