Default Xtreme chrome w/ super gloss clear a no go, again

Yesterday I tried to powdercoat a couple brackets extreme chrome with a super gloss clear coat - put the extreme in the oven @ 400F for all of about 12 mins pulled it out, sprayed the clear, put it in the oven for about another 15 - 20 mins, and it came out a very dulled gray. Last time I fully cured the extreme chrome for 30 mins this time I 1/2 cured it and sprayed the clear on right then. I dunno - I am not having much luck with the clear coat on this powder, which is unfortunate because the extreme chrome looks awesome pre-clear coat.

I redid it with just extreme chrome without clear to see how it holds up - it looks really good so far.