Re: Quadrajet color?
Stra, i just did my Q-jet body a couple days ago, i glass beaded and 1 blowed out all the passages and dipping my body in ruffly a 8% mauratic acid and distilled water for about 10 min. immediately after i took it out and redipped it in plain distilled water bath. after drying it the best i could quickly i then hung it from a 1/2 copper water line over the tank and submerged it into my copy cad tank connected my probes red to anodes and black to copper pipe copper wire . set my amps to 2.5 to 2.7 and my volts where around .8. soaked it for 25 min. and took it out and dipped it into my distilled water bath and then i went to my yellow cad bucket and dipped it in for id say 3 min. rotating by hand. When i took it out into the sun to dry i thought, oh it didn,t work but after about 15 min. the carb. looked factory again. I was told to redip it into the 8% acid tank again but i chanced it. I love the look. Step by step thats what i did!!
|