Re: Nickel Plating Problems After Flash Copper
Hey Mark,
Okay, one last rundown before I dive in here......
Sandblast, degrease, fill pits (where necessary). Sand, degrease, activate, rinse and flash copper. Sand, degrease, activate, rinse then into nickel bath.
|