Default Black Oxide sealer not drying

We have the Black Oxide kit. I have not used it much but I now have decided to use it on all the tools I make and sell. The black looks fine but after it is dipped in the sealer it will not dry but stays slimy. It has been hanging to dry for over 12 hours and it is still wet. If you touch it it smears.
What am I doing wrong?